ill start this off by saying i have a new found respect for welders everywhere
yall niggass be makin dis shit look ez
with that said..
i currently grade my
tack welds a c-
they look like ass but get the job done
i dont know why but i cant get a decent tack weld without using filler.. i suck ass
root pass a c+
came out surprisingly good.. since i dont have to hold the filler rod in the other hand im better able to lay down smooth and consistent beads i used 1/16th tungsten with no filler rod
filler pass an f+
i REALLY should have cleaned the metal after i did the root pass before i did a filler/cap pass
not having a welding table really sucks dick.. and i should have used 3/32nd for the cap/filler pass
right now im waiting for the metal to cool but im confident the next piece i weld up will be better
ill use 3/32nd for the cap pass and ill clean the metal between the root and the cap passes
shitty tack
root pass
filler pass
after cleaning (forgot to clean between root and filler passes.. doh!
tips would be greatly appreciated but if all you want to do is talk shit please post in the cummins discussion thread...